Solution Prep
Equipment and Materials:
- Collect a chemical-resistant beaker for the etching solution.
- Prepare a temperature-controlled hotplate with a magnetic stirrer.
- Monitor the solution's temperature.
Solution Preparation:
- Measure the required volume of hydrogen peroxide
- If needed, dilute the hydrogen peroxide to 30% concentration v/v with deionized water. add to the water.
- Place the beaker containing the solution on a temperature-controlled hotplate with a magnetic stirrer.
- Insert a magnetic stir bar into the solution for even heating.
- Position the temperature probe in the solution without letting it touch the beaker bottom.
Heat to Desired Temperature:
Set the hotplate to a low setting and gradually increase to reach 50°C.
Monitor the temperature closely using the thermometer/probe. Stir the solution continuously to maintain uniform heating.
Maintain Temperature:
Once the solution reaches 50°C, adjust the hotplate settings to maintain a steady temperature.
Verify stability for a few minutes before starting the etching process.
Etching Process:
- Carefully immerse the substrate with the patterned photoresist into the heated solution using tweezers.
- Agitate gently to ensure uniform etching of exposed TiN areas.
After Etching:
- Remove the substrate when the desired thickness is achieved.
- Rinse thoroughly with deionized water to stop the etching process.
- Dry the substrate using a nitrogen gun or in a clean environment.
Cleanup and Disposal:
- Allow the solution to cool before transferring it to an appropriate waste container.